DIN1.5815 35nicr6 Structural Round Steel
Chemcial composition:
Grade | C | Mn | P | S | Si | Cr | Ni |
1.5815 | 0.30- 0.37 | 0.60- 0.90 | 0.025 max | 0.025 max | 0.40 max | 0.80- 1.10 | 1.20- 1.60 |
>>>Heat Treatment: Ultrasonic test: According to SEP 1921-84 Soft Annealing Hardening
Tempering Forging |
|
| >>>Steel Grades DIN1.5815 35NC6 FE-PL62 35NiCr6 |
Mill′s test certificate: EN 10204/3.1 with all relevant data reg. chem. composition, mech. properties and results of testing. | Application: • Crankshafts. • Shafts. • Various gears. • Fasteners etc.
|
Mechanical Properties:
Process | Diameter(mm) | Tensile Strength Rm (Mpa) | Yield Strength Rp0.2 (Mpa) | Elongation A5 (%) | Area Reduction Ratio C (%) | Impact Value Kv (J) Room Temperature | Hardness (HB) |
SOFT ANNEALED | / | / | / | / | / | / | 223 max |
QUENCHED AND TEMPERED | 16 max | 880-1080 | 740 min | 12 min | 40 min | / | 261-318 |
QUENCHED AND TEMPERED | 16-40 | 880-1080 | 740 min | 12 min | 40 min | 35 min | 261-318 |
QUENCHED AND TEMPERED | 40-100 | 780-980 | 640 min | 15 min | 40 min | 35 min | 231-289 |
Contact Information:
FUSHUN SPECIAL STEEL CO., LTD.
Tel: 89-0731-89903933(CHANGSHA, Office)
Fax: +86-0731-89853933
Mobile/Whatsapp: +86-
Skype: summerxn at outlook.com
Website:
Email: Summer at fushunspecialsteel.com